ABS Particles Are Returned Without Impurities
ABS Particles Are Returned Without Impurities
ABS Particles Are Returned Without Impurities
ABS Particles Are Returned Without Impurities

ABS Particles Are Returned Without Impurities

Get Latest Price
Packaging & Delivery
Selling Units : Ton
Picture Example :
Real offer at Vietnam exhibition site
ABS resin particles
Product Description
Black ABS return high gloss impact resistance imported recycled Abs Material impact 13 environmental protection electrical materials 1, good overall performance, high impact strength, chemical stability, good electrical performance.
ABS recycled material
2, good welding with 372 plexiglass, made of two-color plastic parts, and can be chrome plated on the surface, spray paint treatment.
3, with high impact resistance, high heat resistance, flame retardant, enhancement, transparency and other levels.
4, the activity is less than HIPS, better than PMMA, PC, etc., good flexibility.
The emergence of recycled materials in order to sustainable use of materials, there is the emergence of ABS recycled materials, which also reduces waste and guarantees
Protect our environment, the level of regeneration on the city and country is not uniform, according to the requirements of the product can find the right recycled materials to do.
Molding characteristics  Polyformaldehyde
1. Amorphous material, medium activity, large moisture absorption, must be fully dry, the surface requires gloss plastic parts must be preheated and dried for a long time 80-90 degrees,3 hours.
2. Suitable for high material temperature, high mold temperature, but the material temperature is too high and easy to decompose (decomposition temperature is > 270 degrees) for high precision plastic parts, mold temperature is suitable for 50-60 degrees, high gloss. Heat resistant plastic parts, mold temperature is suitable for 60-80 degrees.
3, if you need to solve the water pattern, it is necessary to improve the activity of the material, take high material temperature, high mold temperature, or change the inlet water level and other methods.
4, such as the formation of heat-resistant or flame-retardant grade materials, 3-7 days after the production of the mold surface will remain plastic decomposition, resulting in the mold surface shiny, the mold needs to be cleaned in time, the same
The surface of the mold should increase the exhaust position.Polypropylene

Pro

ABS

Home> Products> PC Or ABS> ABS Particles Are Returned Without Impurities
Send Inquiry
*
*

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send